E46-040 · Welding Process & Distortion · Gas-Shielded Welding · ★★
Insufficient shielding-gas flow let air enter the weld and form porosity
[Mechanism] Insufficient flow lets air enter, forming nitrogen and oxygen porosity.
[Calculation] Insufficient flow raises the porosity rate and weakens the section.
[Design gap] The flow rate was not adjusted.
① Sufficient flow: set the shielding-gas flow per specification to ensure stable shielding
② Check the gas hose for leaks: check the gas hose for leaks to ensure the flow
③ Add a wind shield: add a wind screen to avoid draught interference and ensure shielding
④ Ensure gas purity: use gas of acceptable purity to ensure the shielding effect
⑤ Radiographic porosity check: use RT to check for porosity and detect it early
⑥ Repair porosity: repair the porosity locations to restore the section
⑦ Porosity verification: confirm the porosity has been eliminated by RT
⑧ Standardize process: write the flow-rate requirement into the welding procedure specification (WPS), controlling at the source
GB/T 19867.2-2008 Welding procedure specification for mechanized welding and automatic welding