E46-042 · Welding Process & Distortion · Pressure-Retaining Weld · ★★★
With no surface NDT after welding, micro-cracks went undetected and grew into leaks in service
[Mechanism] Without surface NDT micro-cracks are missed and then propagate into cracks and leaks.
[Calculation] Missed micro-cracks propagate and cause cracking and leakage in service.
[Design gap] No MT or PT was performed.
① Post-weld surface NDT: perform MT or PT surface NDT after welding to check for cracks
② Delayed NDT: re-inspect 24 hours after welding to catch delayed cracks
③ Mark crack locations: mark the crack locations to facilitate repair
④ Repair the cracks: repair the crack locations to restore sealing
⑤ Re-inspect after repair: re-inspect after repair to ensure cleanliness
⑥ Keep reports for traceability: retain the NDT reports for traceability
⑦ NDT verification: confirm the cracks have been eliminated by re-inspection
⑧ Standardize process: write the surface-NDT requirement into the specification, controlling at the source
GB/T 15822.1-2005 Magnetic particle testing