E46-043 · Welding Process & Distortion · Annealed Part · ★★

Problem Description

Re-welding near the weld seam of an annealed part let the thermal cycle soften the annealed zone and lower its strength

Root Cause

[Mechanism] The heat of re-welding reheats the annealed zone and softens it, lowering its strength.
[Calculation] The thermal cycle lowers the strength of the softened zone and reduces its load capacity.
[Design gap] Neither heat avoidance nor re-treatment was applied.

Corrective Solution

① Avoid the softened zone: keep the weld away from the annealed softened zone to avoid re-softening
② Local heat control: control the heat input locally to reduce softening
③ Re-anneal after welding: re-anneal after welding to restore performance
④ Measure hardness: measure hardness to detect softening early
⑤ Reinforce the weak zone: reinforce the softened zone to ensure load capacity
⑥ Qualification strength evaluation: run a procedure qualification to evaluate strength and ensure performance
⑦ Softening verification: confirm softening is under control by hardness measurement
⑧ Standardize process: write the heat-avoidance requirement into the process, controlling at the source

Checklist

Reference

GB/T 19866-2005 General principles for welding procedure specification and qualification