E46-046 · Welding Process & Distortion · Multi-Pass Fillet Weld · ★★
Incomplete interpass slag removal in a fillet weld left slag inclusions that cracked and leaked along the weld leg
[Mechanism] Interpass slag rolls up in the fillet weld, and the slag inclusions weaken it so it cracks along the weld leg.
[Calculation] Slag inclusions reduce the effective weld-leg section, causing cracking and leakage.
[Design gap] The fillet-weld slag was not cleaned.
① Clean fillet-weld slag: remove slag between passes of the fillet weld to keep the interpass zone clean
② Angle-grinder cleanup: clean the weld bead with an angle grinder to keep the surface clean
③ Magnetic-particle slag inspection: use MT to check for slag inclusions and detect them early
④ Repair slag inclusions: repair the slag-inclusion locations to restore the section
⑤ Qualification check: verify interpass cleanliness with a test plate to ensure quality
⑥ In-process inspection: check for slag and correct early
⑦ Slag-inclusion verification: confirm the slag inclusions have been eliminated by MT
⑧ Standardize process: write the slag-removal requirement into the welding procedure specification (WPS), controlling at the source
GB/T 19418-2003 Arc-welded joints in steel - Quality classification of defects