E46-047 · Welding Process & Distortion · Medium-Thick Plate · ★★★
Insufficient preheat on medium-thick plate caused under-bead cracking and leakage
[Mechanism] Insufficient preheat makes the cooling rate too high, cracking under the weld bead.
[Calculation] A preheat below the required value keeps the cooling rate above the limit, causing cracking and leakage.
[Design gap] The preheat temperature was not measured.
① Infrared preheat measurement: measure the preheat temperature with an infrared thermometer to ensure it is sufficient
② Preheat to specification: bring the preheat temperature up to the specification requirement and cool slowly
③ Low-hydrogen filler: use low-hydrogen filler metal to reduce the hydrogen content
④ Control interpass temperature: control the interpass temperature to stabilize quality
⑤ NDT for cracks: use NDT to check for cracks and correct early
⑥ Slow cooling after welding: cool slowly after welding to avoid cold cracking
⑦ Crack-prevention verification: confirm there are no cold cracks by NDT
⑧ Standardize process: write the preheat requirement into the welding procedure specification (WPS), controlling at the source
GB/T 19866-2005 General principles for welding procedure specification and qualification