E46-048 · Welding Process & Distortion · Weldment with Sealing Surface · ★★
Weld spatter adhered to the sealing surface, and the cleanup damaged the surface, so it did not seal tightly and leaked
[Mechanism] Spatter adhered to the sealing surface, and cleanup ground it, causing leakage.
[Calculation] Spatter damage to the surface puts flatness out of tolerance, causing the seal to leak.
[Design gap] The sealing surface was not protected.
① Mask the sealing surface: apply protective masking to the sealing surface to prevent spatter adhesion
② Optimize parameters to reduce spatter: optimize parameters to reduce spatter and keep the surface clean
③ Remove spatter gently: remove spatter gently with a scraper to avoid damaging the surface
④ Measure flatness after cleanup: measure flatness after cleanup and correct early
⑤ Precision-grind the damaged spot: precision-grind the damaged spot to restore flatness
⑥ Pressure test for leaks: perform a pressure test to check the seal and detect problems early
⑦ Protection verification: confirm the requirement is met by flatness measurement
⑧ Standardize process: write the sealing-surface protection requirement into the process, controlling at the source
GB/T 19866-2005 General principles for welding procedure specification and qualification