E46-049 · Welding Process & Distortion · Dissimilar-Metal Pipe · ★★★
In a copper-aluminum dissimilar-metal weld, thermal-expansion mismatch cold-cracked the weld and caused a leak
[Mechanism] The difference in thermal-expansion coefficients makes contraction uneven, cracking the interface.
[Calculation] The expansion mismatch makes the interface stress excessive, causing cold cracking and leakage.
[Design gap] No transition joint or compensation was used.
① Use transition joints: use transition joints between dissimilar metals to ease the thermal-expansion mismatch
② Provide expansion joints: install expansion joints to absorb the thermal-expansion mismatch and reduce stress
③ Fast welding with low heat input: use fast welding with low heat input to reduce stress
④ Control the cooling rate: control the cooling rate so contraction is uniform
⑤ NDT for cracks: use NDT to check for cracks and correct early
⑥ Qualification confirmation: re-qualify to confirm the process is feasible and ensure performance
⑦ Cracking verification: confirm there are no cracks by NDT
⑧ Standardize process: write the transition-joint requirement into the process, controlling at the source
GB/T 19866-2005 General principles for welding procedure specification and qualification