E46-050 · Welding Process & Distortion · High-Strength Steel Weld · ★★★
A high-strength steel weld cooled in air after welding hardened and cold-cracked, causing a leak
[Mechanism] Air cooling hardens the high-strength steel, causing hydrogen cracking.
[Calculation] Air cooling keeps the cooling rate above the critical value, so hardening cracks and leakage occur.
[Design gap] Slow cooling was not applied.
① Asbestos insulation for slow cooling: cool slowly after welding with asbestos or insulating material to avoid hardening
② Sufficient preheat: preheat thoroughly before welding and cool slowly
③ Post-weld hydrogen-removal post-heating: apply a hydrogen-removal post-weld heat treatment to expel hydrogen
④ Low-hydrogen consumables: use low-hydrogen consumables to reduce the hydrogen source
⑤ Delayed crack inspection: perform delayed NDT after welding to check for cold cracks and correct early
⑥ Post-weld heat treatment: apply stress-relief heat treatment to reduce residual stress
⑦ Crack-prevention verification: confirm there are no cold cracks by delayed NDT
⑧ Standardize process: write the slow-cooling requirement into the welding procedure specification (WPS), controlling at the source
GB/T 19866-2005 General principles for welding procedure specification and qualification