E46-074 · Heat Treatment & Stress · Large Gear · ★★
The tooth flanks of a large gear were flame-hardened; the torch head moved unevenly leaving a soft band, and local overheating cracked 2 teeth.
[Mechanism] An uneven travel speed of the flame makes the heating uneven, so soft bands and overheated zones coexist and the overheated zones crack.
[Calculation] Uneven travel makes the temperature difference exceed 150℃, and soft bands and cracks coexist.
[Design gap] Neither the torch speed nor the overlap factor was specified.
① Steady travel speed: specify the travel speed of the flame torch to ensure uniform heating with no soft bands
② Control the overlap: set a proper overlap between adjacent hardened zones to avoid soft bands
③ Control the flame temperature: adjust the oxyacetylene ratio to control the flame temperature and avoid overheating
④ Synchronous cooling: provide synchronous quenching water to ensure the cooling rate
⑤ Crack inspection: inspect the tooth flanks for cracks and soft bands after quenching
⑥ Rework: re-quench or repair-weld teeth with soft bands or cracks
⑦ Quality verification: confirm acceptance by hardness testing and flaw detection
⑧ Standardize process: write the flame-hardening parameters into the process card, controlling at the source
GB/T 5617-2005 Determination of effective depth of hardening after induction or flame hardening of steel