E46-207 · Bonding & Sealing · Hydraulic cylinder · ★★★
The hydraulic cylinder piston was sealed with an O-ring; after assembly it leaked externally even at low pressure, and teardown showed the O-ring was not effectively compressed because the groove depth was too deep, leaving the compression rate insufficient.
[Mechanism] An O-ring seals by the contact stress produced by moderate compression; if the compression rate is too small, the contact stress is insufficient and the medium is extruded through the clearance.
[Calculation] The design compression rate should be 15%~25%, but the over-deep groove gave only 6%, far below what sealing requires.
[Design gap] The groove depth was not designed to the standard, and the compression rate was not checked.
① Design to standard: set the groove depth per GB/T 3452.3 to give a compression rate of 15%~25%
② Select the cross-section: choose the O-ring's cross-section diameter and section size according to the pressure
③ Measure the groove: measure the groove depth before assembly to confirm the compression rate is acceptable
④ Control the clearance: control the fit clearance to avoid extrusion (add a backup ring for high pressure)
⑤ Lubricate to aid assembly: use a little grease to help installation and avoid twisting
⑥ Pressure test: after assembly, perform low- and high-pressure holding tests
⑦ Sealing verification: confirm no external leakage by a pressure-holding test
⑧ Standardize process: write the groove dimensions and compression rate into the drawing
GB/T 3452.3-2005 Rubber O-rings - Groove dimensions