E46-218 · Bonding & Sealing · Pneumatic cylinder · ★★
During repair of a pneumatic cylinder, an O-ring with an undersized cross-section diameter was used by mistake; after installation the compression rate became excessive and the ring was easily extruded through the groove clearance, so it leaked even at low pressure.
[Mechanism] The O-ring cross-section diameter does not match the groove; an undersized cross-section pushes the compression rate above the upper limit and makes the ring easy to extrude under high pressure, so the seal fails.
[Calculation] An undersized cross-section pushes the compression rate above 30%, and the relative extrusion clearance increases, so it leaks even at low pressure.
[Design gap] The repair did not select the cross-section diameter to the original specification, but substituted it at will.
① Follow the spec: select the O-ring strictly by the drawing's cross-section diameter and inner diameter
② Check the compression rate: before assembly, calculate the compression rate to stay within the design range of 15%~25%
③ Control the clearance: keep the fit clearance no greater than 1/10 of the cross-section diameter to prevent extrusion
④ Check the marking: verify that the specification marking on the ring matches the drawing
⑤ Trial fit: trial-fit first to confirm the ring enters the groove smoothly with no interference
⑥ Pressure test: after assembly, run low- and high-pressure tests
⑦ Sealing verification: confirm no leakage by pressure holding
⑧ Standardize process: write the specification and compression rate into the repair card
GB/T 3452.3-2005 Rubber O-rings - Groove dimensions