E46-221 · Bonding and Sealing · PP Plastic Part · ★★
A polypropylene (PP) part was bonded to metal with a structural adhesive without any primer treatment; because PP has an extremely low surface energy and is not wettable, the whole bond face separated after a few days.
[Mechanism] Polyolefins such as PP have an extremely low surface energy and are inert; the adhesive does not wet or react with them, so no effective bond forms.
[Calculation] The bond strength on an untreated PP surface is less than 1 MPa, far below the load-bearing requirement.
[Design gap] No flame or primer activation treatment was done according to the plastic type.
① Surface activation: flame-treat or plasma-treat the PP part to raise its surface energy
② Apply primer: use a dedicated primer to improve wetting and bonding
③ Select the adhesive: choose a modified adhesive that bonds to polyolefins
④ Clean: remove mold release and oil contamination
⑤ Trial: make a sample first to confirm the bond strength
⑥ Strength check: verify with a pull-off test
⑦ Bonding verification: confirm compliance by pull-off force
⑧ Standardize process: write the activation and primer steps into the process card
GB/T 7124-2008 Adhesives - Determination of tensile shear strength (rigid material to rigid material)