E46-224 · Bonding and Sealing · Oil-resistant Sealing · ★★
An ordinary silicone sealant was used to seal the pipeline flanges of a fuel depot; after long-term contact with diesel, the sealant swelled and softened, seeped along the edges, and failed.
[Mechanism] Silicone sealant has poor resistance to oil media; oil penetrates and makes the sealant swell and soften, the sealing contact pressure drops, and it leaks.
[Calculation] After oil immersion the volume swells by more than 30%, and elasticity and strength drop markedly.
[Design gap] No oil-resistant sealant was selected for the medium.
① Select the sealant by medium: for oil media choose an oil-resistant sealant such as nitrile or fluoroelastomer
② Medium-resistance test: first run an oil-immersion swelling test to confirm stability
③ Check certification: confirm the sealant's media compatibility list
④ Control the operating conditions: avoid over-temperature and over-pressure that accelerate degradation
⑤ Replace regularly: replace the seal periodically per its service life
⑥ Leak test: run an oil-pressure test after assembly
⑦ Seal verification: confirm no leakage by the oil-pressure test
⑧ Standardize process: write media compatibility into the selection specification