E46-228 · Bonding and Sealing · Hydraulic Cylinder · ★★
A new O-ring was hooked out of its packaging with a metal hook and scratched; after fitting, the scratch bulged and leaked, and the ring failed during the pressure-hold test.
[Mechanism] A sharp object cuts the seal before installation; in service the cut propagates and forms a leakage path.
[Calculation] A scratch deeper than 10% of the cord diameter already leaks noticeably, and the higher the pressure the faster it fails.
[Design gap] No damage-free handling or installation tools were specified.
① Damage-free handling: take the ring by hand or with soft pliers; never scratch it with a metal hook
② Appearance check: visually check before installation for cuts and burrs
③ Remove sharp edges: round and deburr the bore mouth and groove
④ Apply lubricant: apply a thin film of grease before installation to help the ring into the groove
⑤ Seat correctly: confirm the ring seats smoothly without twisting
⑥ Pressure hold: perform a pressure-hold test after installation
⑦ Sealing verification: confirm no leakage by pressure holding
⑧ Standardize process: write the handling and inspection into the work instruction
GB/T 3452.3-2005 Rubber O-rings - Groove dimensions