E46-229 · Bonding and Sealing · Electronic Component Fixing · ★
Circuit-board components were fixed with dispensed adhesive, but points were skipped along the dispensing path; wherever no adhesive was applied the components loosened and tilted under vibration, and the solder joints cracked in shear.
[Mechanism] A missed dispensing point leaves that component unfixed; under vibration it moves and the solder joint cracks in shear.
[Calculation] A missed-point rate above 10% leaves many components unfixed and markedly lowers reliability.
[Design gap] The dispensing points and path were not specified; the operator went by eye at will.
① Fix the points: dispense at each point specified by the drawing
② Fix the path: plan a continuous dispensing path with no skipped points
③ Controllable amount: use a dispenser to keep the amount consistent at each point
④ Visual check: after dispensing, verify that every point has been applied
⑤ Cure: cure under the specified conditions
⑥ Pull test: sample components and pull-test to confirm they are fixed
⑦ Fixing verification: confirm the components do not come loose by the pull test
⑧ Standardize process: write the dispensing points and path into the process card
GB/T 7124-2008 Adhesives - Determination of tensile shear strength (rigid material to rigid material)