E46-231 · Bonding and Sealing · Valve Packing · ★★
The rubber seal ring in a valve stuffing box had not been replaced for a long time; the rubber had hardened and cracked and lost its elasticity, so it leaked along the stem when the valve was operated, and inspection found the ring brittle and cracked.
[Mechanism] Long-term exposure to heat, oxygen and the medium ages and cross-links the rubber, hardening it; it loses elasticity and resilience, and the sealing contact pressure becomes insufficient.
[Calculation] Aging pushes the compression set past 80%, so the seal can no longer spring back to compensate for wear.
[Design gap] No periodic replacement interval for the seals was specified.
① Replace regularly: replace the rubber seals periodically per their service life
② Check for aging: during maintenance, check the ring for hardening and cracking
③ Choose an aging-resistant grade: select an aging-resistant rubber grade according to the medium and the temperature
④ Avoid high temperature: lower the working temperature at the seal to extend its life
⑤ Records: keep a replacement log for traceability
⑥ Leak test: run a seal test after replacement
⑦ Seal verification: confirm no leakage by the test
⑧ Standardize process: write the replacement interval into the maintenance procedure
GB/T 3452.3-2005 Rubber O-rings - Groove dimensions