E46-232 · Bonding and Sealing · Sight-Glass Bonding · ★★
A Plexiglas sight glass was bonded into a steel housing; when the working temperature rose to 80℃, the large difference in thermal expansion between the two materials pushed the shear stress in the adhesive past its limit, and the edge of the sight glass debonded and leaked.
[Mechanism] The thermal expansion coefficients of metal and plastic differ greatly; a temperature rise creates shear stress at the interface, and once it exceeds the adhesive's allowable value the joint debonds.
[Calculation] The expansion difference between steel and Plexiglas is about 10 times, so an 80℃ temperature difference produces shear stress exceeding the adhesive strength.
[Design gap] The thermal expansion difference was not considered and no flexible adhesive was chosen to compensate.
① Choose a flexible adhesive: for dissimilar-material bonding choose a high-elongation flexible adhesive to compensate for the difference
② Reduce the temperature difference: lower the working temperature difference or add thermal insulation
③ Buffer design: leave expansion clearance in the structure
④ Sample temperature test: run a thermal-cycling sample test to confirm no debonding
⑤ Control the stress: avoid rigid restraint
⑥ Service check: check for debonding after temperature changes
⑦ Bond verification: confirm effectiveness by the thermal-cycling test
⑧ Standardize process: write the compensation measures into the design
GB/T 7124-2008 Adhesives - Determination of tensile shear strength (rigid material to rigid material)