E46-233 · Bonding and Sealing · Gearbox Cover Assembly · ★★
After sealant was applied, the gearbox cover was pressed on before the sealant had dried to touch; the adhesive was squeezed out and lost its continuous layer, and oil seeped from the joint face after filling.
[Mechanism] Pressed before it forms an initial film, the sealant is squeezed and broken up, so it cannot form a continuous sealing layer and leaves a leakage path.
[Calculation] Pressing before tack-dry breaks the adhesive layer over more than 50% of the area, and the seal fails.
[Design gap] Assembly was performed without specifying a tack-dry time.
① Control tack-dry: after applying the sealant, let it stand to tack-dry as instructed before closing the cover
② Close with even pressure: press the cover down evenly without tilting
③ Squeeze-out check: after closing, check that the squeeze-out bead is continuous
④ Dwell: after closing, let it stand to cure before filling oil
⑤ Control the environment: keep temperature and humidity favorable for tack-dry
⑥ Leak test: check for leakage after filling oil
⑦ Seal verification: confirm no leakage by the leak test
⑧ Standardize process: write the tack-dry time into the process