After machining, the joint face of the flat flange had a deep through scratch; even with sealant applied, oil seeped along the scratch, and tightening could not close that channel.
[Mechanism] The through scratch forms a continuous groove; the sealant cannot fill the deep groove, and the medium leaks along it.
[Calculation] Once the scratch is deeper than the sealant can fill it becomes a through channel, and it leaks at a pressure of 0.1MPa.
[Design gap] It was not specified that the joint face must be free of through scratches.
① No through scratches: the joint face must have no deep through scratches
② Fine machining: improve the machining quality to remove tool marks
③ Dressing: sand light scratches to remove any through path
④ Fill: build up deep scratches by welding, grind flat, then seal
⑤ Clean the faces: remove chips and oil before assembly
⑥ Pressure test: run a pressure test after assembly
⑦ Seal verification: confirm no leakage by the pressure test
⑧ Standardize process: write the surface-quality requirement into the drawing
JB/T 7316 Reducers - General technical conditions for assembly