E46-241 · Bonding and Sealing · Automated Dispensing Line · ★★
On an automated two-part adhesive line the metering pump was worn and out of calibration, with too much base resin and too little hardener; the adhesive stayed soft for a long time and the batch parts had insufficient bond strength.
[Mechanism] An inaccurate metering pump shifts the two-part ratio, so cross-linking is incomplete and curing is poor.
[Calculation] Pump wear pushes the mix-ratio deviation to 15%, beyond the allowable ±5%, so the degree of cure is insufficient.
[Design gap] The metering pump was not calibrated periodically.
① Periodic calibration: calibrate the metering pump on schedule to ensure mix-ratio accuracy
② Online monitoring: fit online mix-ratio monitoring with an alarm
③ Sample check: make a cure sample every shift to confirm
④ Test before use: run a test shot at the start of the shift to confirm the ratio
⑤ Maintenance: set up a pump maintenance log
⑥ Strength check: confirm with a strength test
⑦ Bond verification: confirm acceptance by the strength result
⑧ Standardize process: write the calibration interval into the procedure
GB/T 7124-2008 Adhesives - Determination of tensile shear strength (rigid material to rigid material)