E46-249 · Bonding and Sealing · Two-Part Adhesive · ★★
The rod used to take hardener was accidentally dipped into the base-resin drum, contaminating the resin; the whole drum gradually self-polymerized and thickened, and later mixed adhesive did not cure properly.
[Mechanism] Hardener entering the base-resin drum triggers self-polymerization of the resin; its reactivity changes and the later mixing ratio no longer works.
[Calculation] Even a small amount of contamination triggers self-polymerization, and the risk of losing the whole drum is high.
[Design gap] No dedicated dispensing tools; the same utensils were used for base resin and hardener.
① Dedicated tools: use separate dedicated dispensing tools for base resin and hardener
② No cross-dipping: dispensing tools must not be dipped into both drums
③ Cap at once: close the drums promptly after use to prevent contamination
④ Clear labeling: label the two drums distinctly so they are not mixed up
⑤ Sample test: run a small sample test before each batch mix to confirm
⑥ Strength check: perform a strength test
⑦ Bond verification: confirm acceptance by the strength result
⑧ Standardize process: write the dedicated tools into the procedure
GB/T 7124-2008 Adhesives - Determination of tensile shear strength (rigid material to rigid material)