Hammer Forging Folds

E46-327 · Casting & Forging · Hammer Forging · ★★

Problem Description

A hammer forging had surface folds 2mm deep; magnetic particle inspection revealed linear defects along the deformation flow lines.

Root Cause

[Mechanism] A mismatch between feed and reduction makes the surface metal flow back and overlap, forming folds.
[Calculation] When the feed is less than the reduction, the surface tends to fold, and the fold angle grows with the mismatch.
[Design gap] The relationship between reduction and feed was not controlled.

Corrective Solution

① Control feed and reduction: keep the feed greater than the single-pass reduction
② Smooth transitions: give the die ample fillets to avoid flow-back at sharp corners
③ Control temperature: adequate temperature preserves ductility and reduces folding
④ Remove scale: descale before forging to reduce pressed-in defects
⑤ Fold check: magnetic particle inspect the surface, detecting problems early
⑥ Grinding: grind out the folds
⑦ Fold verification: confirm the absence of linear defects by inspection
⑧ Standardize process: write the reduction and feed into the forging card, controlling at the source

Checklist

Reference

GB/T 12361-2016 Steel die forgings - Process