Knowledge Base › Process and Assembly Error Case Study › Insufficient Forging Ratio Causing Porosity

Insufficient Forging Ratio Causing Porosity

E46-326 · Casting & Forging · Main Shaft Forging · ★★★

Problem Description

A main shaft forging had a forging ratio of only 1.5 (should be ≥3); transverse impact energy was low and central porosity was not closed up.

Root Cause

[Mechanism] A small forging ratio means insufficient deformation; the as-cast porosity and dendrites are not fully broken up and welded.
[Calculation] When the forging ratio is below 3, porosity remains, and the transverse properties drop as the ratio falls.
[Design gap] The forging ratio was not guaranteed by the blank size.

Corrective Solution

① Guarantee the forging ratio: ensure a ratio ≥3 based on the cross-section deformation
② Combine drawing out and upsetting: use combined drawing out and upsetting to increase the ratio
③ Control the reduction: a single pass with enough deformation breaks up the porosity
④ Blank calculation: back-calculate the blank size from the forging ratio
⑤ Property check: run a transverse impact test after forging, detecting problems early
⑥ Ultrasonic inspection: check whether the central porosity has closed up
⑦ Forging ratio verification: confirm compliance by properties
⑧ Standardize process: write the forging ratio into the process card, controlling at the source

Checklist

Reference

GB/T 12361-2016 Steel die forgings - Process