Knowledge Base › Process and Assembly Error Case Study › Forging Flow Lines Cut Through

Forging Flow Lines Cut Through

E46-329 · Casting & Forging · Crankshaft Forging · ★★★

Problem Description

Subsequent machining of a crankshaft forging cut through the flow lines, giving poor transverse properties at the loaded areas and early fracture.

Root Cause

[Mechanism] The machining feed direction cuts the flow lines transversely, leaving discontinuous fibers in the load-bearing section.
[Calculation] The higher the flow-line cut ratio, the greater the transverse strength loss, and stress concentration grows with the cut.
[Design gap] Machining and the profile were not planned according to the flow-line direction.

Corrective Solution

① Design along the fibers: orient the forging profile and flow lines along the load direction
② Plan machining: run the cutting passes along the flow lines to cut them as little as possible
③ Choose the forging ratio: an adequate ratio keeps the fibers continuous
④ Control allowance: keep it even to avoid deep local cuts
⑤ Flow line check: section a part to inspect flow-line direction, detecting problems early
⑥ Property check: verify performance at the loaded areas
⑦ Fiber verification: confirm the flow lines are continuous
⑧ Standardize process: write the flow-line requirements into the process specification, controlling at the source

Checklist

Reference

GB/T 12361-2016 Steel die forgings - Process