Knowledge Base › Process and Assembly Error Case Study › Improper Cooling After Hot Forging Causing Cracks

Improper Cooling After Hot Forging Causing Cracks

E46-330 · Casting & Forging · High-Carbon Steel Forging · ★★★

Problem Description

After stack cooling, a high-carbon steel forging showed surface cracks 20mm long, and a flake-sensitive steel developed internal flakes after forging.

Root Cause

[Mechanism] An improper cooling rate builds high residual stress, or hydrogen has no time to diffuse and forms flake cracks.
[Calculation] Too fast a cooling rate lets stress exceed the strength and crack the part, while insufficient slow cooling leaves hydrogen to collect into flakes.
[Design gap] Slow cooling and dehydrogenization after forging were not specified.

Corrective Solution

① Slow cooling: after forging, place parts in a slow-cooling pit or holding furnace
② Dehydrogenization: isothermally dehydrogenize flake-sensitive steel
③ Control stack cooling: avoid stacking that dissipates heat unevenly
④ Upstream hydrogen control: control hydrogen in melting to reduce the source
⑤ Crack check: magnetic particle and ultrasonic inspect after forging, detecting problems early
⑥ Slow-cooling monitoring: record the cooling curve to confirm
⑦ Cooling verification: confirm the absence of cracks and flakes by inspection
⑧ Standardize process: write the cooling specification into the process card, controlling at the source

Checklist

Reference

JB/T 5073-1991 Heat treatment of forgings