Wrong Forging Direction Breaking Up Fiber Flow

E46-333 · Casting & Forging · Gear Blank Forging · ★★★

Problem Description

The forging flow lines of a gear blank ran radially, so the fibers were cut where the tooth root carries load, cutting bending fatigue life by 30%.

Root Cause

[Mechanism] The upsetting and drawing directions leave the flow lines not following the gear rim circumference, so the fibers are discontinuous at the tooth root.
[Calculation] A large angle between the flow lines and the principal stress lowers fatigue strength; fibers oriented tangentially are best.
[Design gap] The flow lines were not planned to run tangentially around the gear rim.

Corrective Solution

① Plan the flow lines: use upsetting and drawing so the fibers run tangentially around the rim
② Radial upsetting: use radial forging or ring rolling
③ Control the sequence: upset first, then punch, then expand
④ Flow line check: section a part to inspect fiber direction, detecting problems early
⑤ Property check: verify with bending fatigue testing
⑥ Profile optimization: make the tooth profile continuous along the fibers
⑦ Fiber verification: confirm the flow lines run tangentially
⑧ Standardize process: write the flow-line planning into the process specification, controlling at the source

Checklist

Reference

GB/T 12361-2016 Steel die forgings - Process