Scale Pressed In During Heating

E46-335 · Casting & Forging · Forging · ★★

Problem Description

The forging surface had scale pits pressed in 0.5mm deep; magnetic particle inspection revealed point-like defects and more fatigue origins.

Root Cause

[Mechanism] Scale formed during heating is not removed and is pressed into the surface during forging, forming pits and inclusions.
[Calculation] Scale thickness grows with heating temperature and time, and pressed-in defects grow with the fraction left uncleaned.
[Design gap] No descaling operation was provided.

Corrective Solution

① Provide descaling: high-pressure water descale after heating and before forging
② Control furnace atmosphere: adjust the atmosphere to reduce oxidation
③ Reduce soaking: shorten the high-temperature soaking time
④ Surface check: inspect for scale pits after forging, detecting problems early
⑤ Grinding: grind out the pits
⑥ Magnetic particle inspection: check for pressed-in inclusions
⑦ Descaling verification: confirm the absence of pressed-in defects by surface inspection
⑧ Standardize process: write the descaling operation into the process card, controlling at the source

Checklist

Reference

GB/T 12361-2016 Steel die forgings - Process

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL