Low Die Temperature in Aluminum Alloy Forging

E46-336 · Casting & Forging · Aluminum Alloy Forging · ★★★

Problem Description

An aluminum alloy forging had a die temperature of only 150℃ (should be 300℃), causing incomplete filling and surface cracks.

Root Cause

[Mechanism] A low die temperature chills the metal on contact; poor flow leaves filling incomplete and cracks the surface layer.
[Calculation] Below the critical die temperature the contact cooling rate rises sharply, and cracking grows with the temperature difference.
[Design gap] The die was not preheated to working temperature.

Corrective Solution

① Preheat the die: preheat the die to a working temperature of about 300℃
② Control die temperature: keep the die temperature even during forging
③ Match billet temperature: match the billet temperature to the die temperature
④ Proper lubrication: use graphite or a dedicated lubricant
⑤ Filling check: inspect for filling and cracks on die opening, detecting problems early
⑥ Adjust the process: raise the die temperature and reforge
⑦ Die temperature verification: confirm crack-free filling
⑧ Standardize process: write the die temperature into the process card, controlling at the source

Checklist

Reference

GB/T 13320-2007 Steel die forgings - Grain size

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »