E46-338 · Casting & Forging · Open-Die Square Bloom · ★★
During open-die drawing out, the square bloom was turned improperly; its cross-section became flattened and diamond-shaped, and positioning in later die forging was off.
[Mechanism] A wrong turning sequence during drawing out distorts the cross-section, and misaligned edges make it diamond-shaped.
[Calculation] An error in the turning angle compresses the opposite corners unevenly, and distortion grows with erratic turning.
[Design gap] The turning sequence and angle were not specified.
① Define the turning sequence: turn in 90° steps during drawing out
② Control feed: keep the feed uniform to prevent drift
③ Check the section: measure the diagonals each pass to prevent distortion
④ Use shaped dies: use shaped dies to true up the section when necessary
⑤ Section check: measure the diagonals, detecting problems early
⑥ Truing: return distorted sections to the furnace and reforge
⑦ Section verification: confirm squareness by dimensions
⑧ Standardize process: write the turning sequence into the forging card, controlling at the source
GB/T 15826-1995 Steel open-die forgings on hammers - Process