Excessive Die Forging Flash Wasting Material

E46-339 · Casting & Forging · Die Forging · ★★

Problem Description

A die forging had flash thickness over 8mm (should be ≤4mm), which wasted material and made trimming difficult and prone to scoring.

Root Cause

[Mechanism] An oversized billet or insufficient press tonnage forces the excess metal out into thick flash.
[Calculation] Flash thickness grows with billet excess and insufficient tonnage, and over-thick flash raises trimming stress.
[Design gap] The billet volume was not optimized.

Corrective Solution

① Optimize billet volume: size the billet precisely from the die cavity to cut the excess
② Raise press tonnage: adequate tonnage keeps the flash thin
③ Control temperature: adequate temperature aids metal flow
④ Check flash: measure flash thickness on mold opening, detecting problems early
⑤ Trimming check: inspect for scoring after trimming
⑥ Adjust the process: reduce the billet or raise the tonnage and reforge
⑦ Flash verification: confirm compliance by thickness
⑧ Standardize process: write the billet volume into the process card, controlling at the source

Checklist

Reference

GB/T 12361-2016 Steel die forgings - Process

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL