E46-341 · Casting & Forging · Steel Casting · ★★★
The riser of a steel casting was not cut until the day after pouring; the casting cracked during removal, with cracks following the hot spot.
[Mechanism] Cutting the riser before stress relief lets residual stress release abruptly and crack the casting.
[Calculation] Residual stress grows with uneven cooling; cutting the riser without annealing lets the stress exceed the strength and crack it.
[Design gap] Stress relief was not performed before riser removal.
① Stress relief first: anneal to relieve stress before cutting the riser
② Control removal: cut symmetrically with a torch or grinding wheel to reduce stress
③ Slow cooling: slow-cool after removal
④ Check for cracks: magnetic particle inspect after removal, detecting problems early
⑤ Stress measurement: measure residual stress by the hole-drilling method when necessary
⑥ Weld repair: gouge out the cracks to sound metal and weld repair
⑦ Removal verification: confirm the absence of cracks by inspection
⑧ Standardize process: write the pre-riser-removal sequence into the process route, controlling at the source
JB/T 50164-2016 Heat treatment specifications for iron castings