E46-364 · Surface Treatment & Coating · Powder-coated part · ★
The powder-coated part showed orange peel and pitting on its surface; clumps in the powder clogged the gun because the powder had not been sieved and had absorbed moisture.
[Mechanism] Powder clumps make atomization and deposition uneven, producing orange peel and pitting.
[Calculation] When the powder particle size exceeds 100μm the clumping rate rises, and poor atomization produces orange peel.
[Design gap] Powder sieving, humidity control and fluidization were not applied.
① Sieve the powder: sieve every shift to remove clumps and keep the particle size even
② Control humidity: keep the powder bin below 45% humidity to prevent clumping
③ Even fluidization: use a fluidized bed to feed the powder evenly and stabilize atomization
④ Orange-peel check: inspect the panel surface for orange peel and detect problems early
⑤ Re-spray: sand and re-spray orange-peeled parts to restore smoothness
⑥ Control the gun: set gun distance and voltage according to the powder to ensure atomization
⑦ Appearance verification: confirm absence of orange peel by visual inspection, confirmed by data
⑧ Standardize process: write sieving and humidity control into the powder specification, controlling at the source
GB/T 21782.1-2008 Coating powders - Part 1