E46-366 · Surface Treatment & Coating · Electroless nickel-plated part · ★★
The electroless nickel-plated part had a large film-thickness variation with local unplated areas; bath pH and temperature fluctuation was not controlled, so deposition was unstable.
[Mechanism] Fluctuations in pH and temperature make the reduction rate unstable, so the coating thickness is uneven.
[Calculation] For every 5℃ drop in temperature the deposition rate falls about 20%, and the film-thickness variation exceeds tolerance.
[Design gap] Continuous temperature control, pH control and stirring were not applied.
① Control temperature: keep the bath temperature steady at 90℃ to ensure even deposition
② Control pH: hold pH at 4.5-5.0 with continuous replenishment to keep the reaction stable
③ Stir vigorously: circulate and stir to prevent concentration gradients and keep deposition even
④ Film-thickness check: use thickness measurement to check even thickness and detect problems early
④ Re-plate: strip and re-plate uneven parts to restore uniformity
⑤ Control loading: keep the loading volume suitable to maintain the ratio and prevent fluctuation
⑥ Thickness verification: confirm even distribution by thickness measurement, confirmed by data
⑦ Standardize process: write temperature and pH control into bath management, controlling at the source
GB/T 13913-2008 Metallic coatings - Electroless nickel-phosphorus alloy coatings