Missed Coatings on Edges and Corners, Rusting

E46-375 · Surface Treatment & Coating · Steel structure inner corner · ★★

Problem Description

The steel structure's inner corners and the area under bolt heads rusted within a year; the spray coating missed edges and corners, so the film was thin.

Root Cause

[Mechanism] Atomized spray rebounds at edges and corners, leaving a thin film that becomes a corrosion source.
[Calculation] The edge film thickness is only 40% of that on flat surfaces, so it rusts first.
[Design gap] Edges and corners were not pre-coated or touch-up coated.

Corrective Solution

① Pre-coat the edges: brush-coat edges and corners before spraying to ensure film coverage
② Touch-up spray: give edges and corners a second spray to build thickness
③ Control gun angle: spray the inner corner at an angle to reduce rebound
④ Edge check: check the film thickness at edges and corners to detect problems early
⑤ Touch-up: touch up thin areas to restore the barrier
⑥ Control gun travel: move slowly in inner corners to ensure coverage and prevent misses
⑦ Film-thickness verification: confirm adequate edge thickness by measurement, confirmed by data
⑧ Standardize process: write edge pre-coating into the process, controlling at the source

Checklist

Reference

GB/T 30790.1-2014 Paints and varnishes - Protective coating systems