Knowledge Base › Process and Assembly Error Case Study › Impurities in Electrophoretic Bath, Rough Film

Impurities in Electrophoretic Bath, Rough Film

E46-374 · Surface Treatment & Coating · Electrophoretic coated part · ★★

Problem Description

The electrophoretic film was rough with many particles; mechanical impurities and oil in the bath were not filtered out, so the film surface was poor.

Root Cause

[Mechanism] Bath impurities attach to the workpiece and form particles, leaving a rough film prone to pitting.
[Calculation] When impurities exceed 50mg/L the particle rate rises and the film surface degrades.
[Design gap] Continuous filtration and oil removal were not applied.

Corrective Solution

① Continuous filtration: circulate the bath through filter bags to remove impurities
② Oil removal: add an oil-removal unit to control oil and prevent adhesion
③ Control parameters: keep pH and conductivity steady to stay clean
④ Particle check: section a sample to check for particles and detect problems early
⑤ Re-deposit: sand and re-deposit rough-film parts to restore gloss
⑥ Control pretreatment: clean pretreatment to prevent carry-over contamination and keep it clean
⑦ Film-surface verification: confirm absence of particles by visual inspection, confirmed by data
⑧ Standardize process: write the filtration frequency into bath management, controlling at the source

Checklist

Reference

GB/T 13492-1992 Automotive topcoats in various colors