E46-373 · Surface Treatment & Coating · Hot-dip galvanized part · ★
The hot-dip galvanized part showed white rust after storage; the passivation film had not formed or was damaged, so the zinc corroded white.
[Mechanism] Improper passivation leaves the zinc surface unprotected, and under moisture it forms basic zinc carbonate white rust.
[Calculation] Without passivation the white-rust rate on the zinc layer rises several-fold and appears during storage.
[Design gap] Passivation was not done, or was not dried after passivation.
① Passivate: passivate with chromium or trivalent chromium after galvanizing to preserve the film
② Control drying: dry thoroughly after passivation to prevent residual liquid
③ Control storage and transport: store dry and ventilated to prevent stacked moisture
④ White-rust check: check the surface for absence of white rust to detect problems early
⑤ Re-passivate: derust and re-passivate white-rusted parts to restore protection
⑥ Control packaging: use paper interleaving to prevent moisture in stacks and stay dry
⑦ Corrosion-protection verification: confirm absence of white rust after storage, confirmed by data
⑧ Standardize process: write passivation into post-galvanizing treatment, controlling at the source
GB/T 13912-2020 Metallic coatings - Hot dip galvanized coatings on fabricated iron and steel articles