E46-372 · Surface Treatment & Coating · Multi-coat part · ★★
Adhesion between the multiple coats was low and they peeled off in sheets; the intercoat surface was smooth and unground, so the interface was weak.
[Mechanism] The intercoat surface is smooth and overcured, so the next coat cannot key in and the interface bond is weak.
[Calculation] With high intercoat gloss and no sanding, adhesion drops by about 40%.
[Design gap] Intercoat sanding or a transition coat was not specified.
① Intercoat sanding: lightly sand after the previous coat is surface-dry to increase roughness
② Control the interval: set the sanding time by when the coat is surface-dry to keep it suitable
③ Transition coat: use a transition paint to bridge the coats for strong bonding
④ Adhesion check: use an intercoat cross-cut test to detect problems early
⑤ Re-coat: sand and redo delaminated parts to restore intercoat bonding
⑥ Control film thickness: keep each coat from being too thick to prevent slip
⑦ Adhesion verification: confirm stability by cross-cut testing, confirmed by data
⑧ Standardize process: write intercoat sanding into the process, controlling at the source
GB/T 30790.1-2014 Paints and varnishes - Protective coating systems