E46-378 · Surface Treatment & Coating · Powder-coated part · ★

Problem Description

Parts from the same powder lot showed obvious color differences; powder lots were mixed and curing temperature and time varied, so the color was unstable.

Root Cause

[Mechanism] Differences in pigments between powder lots and uneven oven temperature make the shade inconsistent.
[Calculation] A 10℃ oven temperature difference gives a color difference ΔE above 1.5, visible to the eye.
[Design gap] Same-lot powder, same-oven curing and temperature control were not applied.

Corrective Solution

① Same powder lot: use powder from the same lot number for the same part to ensure color
② Control oven temperature: keep the oven temperature even and steady to reduce variation
③ Control time: keep curing time adequate and consistent for proper cure
④ Color-difference check: use a colorimeter to check for ΔE≤1.5 and detect problems early
⑤ Re-coat: re-spray off-color parts with the same lot to restore uniformity
⑥ Control film thickness: keep the film thickness even to prevent depth-of-color differences
⑦ Color-difference verification: confirm meeting spec with a colorimeter, confirmed by data
⑧ Standardize process: write same-lot, same-oven into the powder process, controlling at the source

Checklist

Reference

GB/T 21782.1-2008 Coating powders - Part 1