Knowledge Base › Process and Assembly Error Case Study › Poor Coating Adhesion, Peeling

Poor Coating Adhesion, Peeling

E46-379 · Surface Treatment & Coating · Electroplated part · ★★

Problem Description

The electroplated part's coating peeled off when bent; pretreatment was unclean or the current was too high, so the coating was loose.

Root Cause

[Mechanism] Oil and oxidation on the substrate leave the coating unbonded, so it peels as soon as the part bends.
[Calculation] Residual oil from pretreatment lowers adhesion by 80%, so it peels easily.
[Design gap] Pretreatment and current density were not controlled.

Corrective Solution

① Clean pretreatment: degrease and acid-clean before plating to preserve adhesion
② Control current: keep current density within spec to prevent burning and loosening
③ Control activation: activate before plating to keep the surface active and improve bonding
④ Bond check: use bending or thermal shock to check peeling and detect problems early
⑤ Re-plate: strip and re-plate peeled parts to restore bonding
⑥ Control the plating bath: keep the bath clean against contamination to preserve quality
⑦ Bond verification: confirm no peeling by bending, confirmed by data
⑧ Standardize process: write pretreatment into the plating process, controlling at the source

Checklist

Reference

GB/T 9799-2011 Metallic coatings - Electroplated coatings of zinc on iron or steel

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »