Poor Sealing in Anodizing, Loss of Gloss

E46-381 · Surface Treatment & Coating · Anodized aluminum part · ★★

Problem Description

After anodizing the aluminum part's surface powdered and lost gloss; poor sealing let the film adsorb dirt.

Root Cause

[Mechanism] Insufficient sealing leaves the oxide film porous and it adsorbs dirt, losing gloss and powdering.
[Calculation] The sealing rate should be ≥98%; below that it adsorbs dirt and loses gloss.
[Design gap] The sealing temperature, time and pH were not controlled.

Corrective Solution

① Control sealing: hot-water seal at 95℃ held for 15 minutes for complete sealing
② Control pH: keep the sealing bath at pH 5.5-6.5 to preserve quality
③ Choose the medium: use nickel salt sealing to improve corrosion resistance and stability
④ Sealing check: use the dye-stain test to check the sealing rate and detect problems early
⑤ Re-seal: re-seal poor parts to restore dirt resistance
⑥ Control pre-anodizing: let the oxide film be even before sealing to ensure effectiveness
⑦ Sealing verification: confirm ≥98% by dye-stain testing, confirmed by data
⑧ Standardize process: write the sealing parameters into the anodizing process, controlling at the source

Checklist

Reference

GB/T 8013.1-2018 Anodic oxide coatings on aluminium and aluminium alloys