E46-386 · Surface Treatment & Coating · Chemically oxidized aluminum part · ★
After chemical oxidation the aluminum part had poor conductivity and corrosion resistance; the film was only 0.5μm (should be 2μm) because the bath concentration was low.
[Mechanism] Low oxidizing-bath concentration and low temperature make the film thin, so protection is poor.
[Calculation] Halving the concentration halves the film thickness; 0.5μm is insufficient.
[Design gap] The bath concentration and temperature were not controlled.
① Control concentration: keep the oxidizing bath at its standard concentration to ensure the film
② Control temperature: keep the bath at a steady 30℃ for adequate film formation
③ Control time: allow enough immersion time to ensure thickness
④ Film check: use thickness measurement to check for ≥2μm, detecting problems early
⑤ Re-oxidize: re-oxidize thin-film parts to restore corrosion resistance
⑥ Control pretreatment: degrease cleanly before oxidizing to preserve adhesion
⑦ Film-thickness verification: confirm meeting spec by thickness measurement, confirmed by data
⑧ Standardize process: write concentration and temperature into the oxidation process, controlling at the source
GB/T 17460-1998 Chemical conversion coatings - Rinsing on aluminum and aluminum alloys