Knowledge Base › Process and Assembly Error Case Study › Electrophoretic Part Energized on Entry, Pinholes

Electrophoretic Part Energized on Entry, Pinholes

E46-395 · Surface Treatment & Coating · Electrophoretic part · ★★

Problem Description

The electrophoretic part was energized as it entered the tank, arcing and causing pinholes; the power was not cut before immersion, so the coating broke down.

Root Cause

[Mechanism] Energized entry makes the local current density too high, causing arcing and pinholes.
[Calculation] A large voltage difference on entry punctures the film, and the pinholes expose the substrate.
[Design gap] The part was not immersed with the power off and allowed to settle.

Corrective Solution

① Cut the power: switch off and let the part settle before immersion to prevent arcing
② Control immersion: energize only after the part is fully immersed for stable deposition
③ Control voltage: raise the voltage slowly to prevent breakdown
④ Check pinholes: section a sample to inspect for pinholes, detecting problems early
⑤ Re-deposit: sand and re-deposit pinhole parts to restore coverage
⑥ Control the bath: keep the tank bath parameters steady for uniformity
⑦ Film-thickness verification: confirm no exposed substrate by thickness measurement, confirmed by data
⑧ Standardize process: write power-off immersion into the electrophoretic process, controlling at the source

Checklist

Reference

GB/T 13492-1992 Automotive topcoats in various colors

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL