Knowledge Base › Process and Assembly Error Case Study › Poor Coating Adhesion from Oily Substrate

Poor Coating Adhesion from Oily Substrate

E46-394 · Surface Treatment & Coating · Machined part · ★★

Problem Description

The coating peeled off in whole sheets; the machining oil on the substrate had not been removed, so the interface did not adhere.

Root Cause

[Mechanism] The machining oil film blocks bonding, so the coating peels off in whole sheets.
[Calculation] Residual oil brings adhesion close to 0, causing complete peeling.
[Design gap] Neither degreasing nor sanding/roughening was done.

Corrective Solution

① Clean degreasing: degrease cleanly with solvent or alkali to keep it clean
② Roughen the surface: sand or blast to increase roughness and improve adhesion
③ Choose a primer: use a strongly adhering primer to ensure bonding
④ Adhesion check: use a cross-cut test to check adhesion and detect problems early
⑤ Re-coat: clean and redo peeled parts to restore bonding
⑥ Control the source: prevent renewed oil contamination and keep it clean
⑦ Adhesion verification: confirm Grade 1 by cross-cut testing, confirmed by data
⑧ Standardize process: write degreasing and roughening into pretreatment, controlling at the source

Checklist

Reference

GB/T 8923.1-2011 Preparation of steel substrates before application of paints

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »