E46-393 · Surface Treatment & Coating · Hot-dip galvanized part · ★
Galvanized parts stacked in the warehouse developed white rust; poor ventilation let moisture condense and the zinc corroded white.
[Mechanism] Stacking with poor ventilation traps moisture, and white rust forms on the zinc surface.
[Calculation] Stacking at a relative humidity above 60% produces white rust and degrades storage.
[Design gap] Warehouse ventilation and interleaving were not controlled.
① Ventilated storage: ventilate the warehouse to reduce humidity and prevent condensation
② Interleave: place paper between parts for ventilation to prevent trapped moisture
③ Control humidity: keep humidity ≤60% to stay dry
④ White-rust check: check for absence of white rust to detect problems early
⑤ Remove white rust: derust and passivate white-rusted parts to restore protection
⑥ Wrap for protection: apply protection for long-term storage to preserve the surface
⑦ Corrosion-protection verification: confirm by absence of white rust, confirmed by data
⑧ Standardize process: write the storage requirements into post-galvanizing, controlling at the source
GB/T 13912-2020 Metallic coatings - Hot dip galvanized coatings on fabricated iron and steel articles