E46-397 · Surface Treatment & Coating · Equipment markings · ★

Problem Description

The equipment's warning markings blurred and peeled off; the marking was applied before the paint dried or the substrate adhesion was poor.

Root Cause

[Mechanism] The marking paint was not dry or the substrate was untreated, so adhesion was poor and the marking blurred and peeled.
[Calculation] Marking applied before drying smears the characters, and insufficient adhesion causes peeling.
[Design gap] Marking paint curing and substrate treatment were not controlled.

Corrective Solution

① Clean the substrate: degrease cleanly before marking to preserve adhesion
② Control drying: apply the marking only after the paint is fully dry to prevent smearing
③ Choose the paint: use a marking-specific paint for greater durability
④ Legibility check: check that the characters are clear to detect problems early
⑤ Re-mark: clean and re-mark blurred parts to restore legibility
⑥ Control film: keep the marking film moderate to prevent build-up
⑦ Legibility verification: confirm legibility by visual inspection, confirmed by data
⑧ Standardize process: write the marking process into coating, controlling at the source

Checklist

Reference

GB/T 2893.1-2013 Graphical symbols - Safety colours and safety signs