Coating Internal Stress Cracking

E46-398 · Surface Treatment & Coating · Thick nickel-plated part · ★★

Problem Description

A thick nickel-plated part cracked in storage; the coating had high internal stress and was thick, so it cracked on its own.

Root Cause

[Mechanism] A thick coating accumulates stress beyond its strength and cracks by itself.
[Calculation] Above 50μm the nickel layer's stress surges and it cracks.
[Design gap] Coating thickness and additives were not controlled.

Corrective Solution

① Control thickness: keep the nickel layer ≤50μm to reduce stress
② Additives: use a stress-reducing additive to lower internal stress
③ Control temperature: keep the plating bath temperature steady to preserve quality
④ Crack check: check for absence of cracks to detect problems early
⑤ Re-plate: strip and re-plate cracked parts to restore integrity
⑥ Control pretreatment: clean pretreatment to preserve adhesion
⑦ Thickness verification: confirm compliance by thickness measurement, confirmed by data
⑧ Standardize process: write the plating thickness into the plating process, controlling at the source

Checklist

Reference

GB/T 9798-2005 Metallic coatings - Electrodeposited coatings of nickel