E46-403 · Commissioning & Run-In · Motor bearing · ★★★
After servicing, the bearing inner ring was hammered directly with a brass bar onto the motor shaft; in service the inner ring developed a circumferential crack, shattered and seized.
[Mechanism] Hammering subjects the inner ring to impact bending, and the local stress exceeds the material yield, producing microcracks.
[Calculation] The impact force far exceeds a press-fit force, and the stress concentration at the inner-ring wall exceeds the limit.
[Design gap] Neither heating nor hydraulic press tooling was used for the fit.
① Heat-fit: heat the bearing to 80℃ to 100℃ and slip it on while hot to avoid impact
② Dedicated tooling: press on the inner ring alone with a sleeve, or press evenly with a hydraulic press so force is not transmitted to the outer ring
③ Control temperature: keep the heating temperature below 120℃ to prevent the bearing from annealing and softening
④ Measure the fit: before assembly measure the interference between the shaft journal and inner ring and confirm it is within design range
⑤ Listen in operation: after assembly run it unloaded and listen for abnormal noise; if present, disassemble and inspect
⑥ Verify torque: confirm the lock-nut torque meets spec to prevent axial play
⑦ Quality verification: confirm assembly acceptance by temperature rise and absence of abnormal noise, confirmed by data
⑧ Standardize process: write heat fitting into the service process, controlling at the source
GB/T 307.1-2017 Rolling bearings - Radial bearings - Tolerances