E41-496 · Motor Selection · Motor Bearing-Bore Wear Spinning-in-Housing · ★★★
In a 10-year-old motor, the front-end-cover bearing bore wore about 0.1 mm; the bearing outer race turned within the bore (spinning in housing), producing abnormal friction noise and high temperature.
The bearing bore (Φ110H7, +0.035/0) in the motor front end cover (HT200 cast iron) wore over 10 years of use as the bearing outer race fretted against it. The wear rate is about 0.01 mm/year, totaling about 0.1 mm over 10 years (measured bore Φ110.12 mm). The fit between outer race and bore changed from the original transition fit (max clearance 0.01 mm) to a clearance fit (clearance about 0.085 mm). The outer race creeps within the clearance (spins in housing); its surface rubs the bore wall, generating friction heat and noise. Abrasive iron powder enters the bearing and accelerates raceway wear. The spinning outer race also offsets the rotor radially, making the motor air gap uneven (gap difference grows from 0.05 mm to 0.12 mm), creating a unilateral magnetic pull that worsens vibration.
① Repair worn motor bearing bore: insert a sleeve (steel sleeve 3 mm thick, interference fit pressed in) → re-bore to standard size\n② Or apply bearing retainer adhesive (Loctite 641, fills clearance ≤0.25 mm)\n③ Prefer an interference fit (J6/js6) between outer race and bore\n④ Periodically check bearing-bore size (every 3 years; repair if wear >0.03 mm)\n⑤ Replace the motor end cover (replace directly when the bore is severely worn)
FT_12 Systematic Motor Selection