E41-339 · Screw Selection · Domestic-Substitute Screw Wear · ★★★★
After 6 months of use, the domestic-substitute screw (C3 class) degraded in accuracy from ±0.005mm/300mm to ±0.015mm/300mm. Inspection found the screw raceway surface hardness was only HRC55 (required ≥HRC58).
The screw raceway surface should be induction-hardened, with a hardened case depth ≥1mm and surface hardness HRC58~62. The domestic substitute screw used improper induction-hardening parameters (insufficient power or too-short heating time), so its actual case depth was only 0.5mm and surface hardness HRC55. Insufficient hardness caused the raceway to undergo plastic deformation under cyclic stress (running-in wear); the wear rate W=K×σ×v/hardness. At HRC55 the wear rate is 2× that at HRC60 (wear rate is inversely proportional to hardness). After 6 months the raceway wear depth was about 0.005mm, and the cumulative lead error grew from ±0.005mm to ±0.015mm. Meanwhile the screw fatigue life L∝(HRC/HRC_rated)^3=(55/60)^3≈0.77, a 23% reduction.
① Check screw raceway hardness: use a Leeb hardness tester (HLD) at the unthreaded end\n② Standard requirement: surface hardness HRC58~62, hardened case depth ≥1mm\n③ The domestic-screw supplier must provide heat-treatment parameters (quench temperature/time/medium)\n④ Incoming inspection: sample 3 pieces per batch for hardness (reject and replace if failing)\n⑤ Use branded screws (HIWIN/Yintai/THK, controllable quality)
FT_11 Ball Screw Selection