E41-347 · Screw Selection · Screw Bearing Spring Preload Failure · ★★★★
The preload spring (disc-spring pack) of the screw-support bearing fractured after 2 years; the bearing lost preload and the screw had about 0.02mm axial play.
The fixed-end bearing set is preloaded by disc springs (Series A, OD 80mm, ID 41mm, thickness 2mm, 10 pieces in parallel-stack). The springs are compressed to 0.6h₀ (h₀=1.6mm as the limit travel) under preload, with a preload force about 800N. Under sustained compressive stress the disc springs relaxed; after 2 years the free height dropped from 60mm to 58mm (1.5% compressive deformation). The pre-compression fell from 0.6h₀ to 0.5h₀, and preload from 800N to about 500N. The bearing-set axial stiffness K∝F_pre, so a 37.5% preload drop lowered stiffness about 37.5%. Under a 3000N cutting force the screw axial displacement grew from δ=3000/2000=1.5μm to δ=3000/1250=2.4μm. More seriously, the springs developed fatigue cracks under alternating stress (small rolling defects on the spring surface) that propagated to fracture.
① Periodically check disc-spring pack preload (once a year, measure with a dynamometer)\n② Check spring free height (replace when below 95% of original)\n③ Upgrade spring material: 60Si2MnA → 50CrVA (fatigue strength up 30%)\n④ Spring surface shot-peening + phosphating (fatigue life up 2×)\n⑤ Or switch to a cylindrical coil spring (more uniform stress, longer life)
FT_11 Ball Screw Selection